Cast 281F tin/bismuth, inside 550F pewter molds? 2 Years ago
|
|
|
I am wondering if any of you have tried casting 281F tin/bismuth; inside molds made of pewter. These pewters like Rotometals A/C and Hallmarks 92-8 melt at over 400F. Where 281F should melt at about 281F. I haven't any experience with those materials as yet. I am also wondering if they would release from one another without a parting agent.
|
|
|
Logged
|
|
|
Last Edit: 2010/02/01 20:35 By Stephen Casey.
|
|
|
The administrator has disabled public write access.
|
|
|
Re:Cast 281F tin/bismuth, inside 550F pewter molds? 2 Years ago
|
|
|
I have just started playing with Bismuth and haven't tried any of the low melt alloys. I would like to get some Tin but the budget won't handle it for now. Too cold outside to do anything so I'm just working on inside projects.
|
|
Jammer (Moderator)
Administrator
Posts: 915
|
Logged
|
|
|
The administrator has disabled public write access.
|
|
|
|
|
|